Designed for measurement of thermophysical properties, the MP-V offers multiple methods for primary measurement of solids, liquids, paste and powders. With intelligent transient parameter automation, measurements are expertly performed.
MP-V Specifications:
• High sensitivity controller, with Wheatstone Bridge
• Data-Point Collection (points): 400 to 600
• MP software packages: Testing and Analysis
• iTransient Parameter Automation
• Unlimited online Training and Support from Thermtest Service Engineer
Thermal Conductivity Methods Included:
• Transient Plane Source (TPS) Method for testing the absolute thermal conductivity, thermal diffusivity, specific heat and thermal effusivity of solids, pastes & powders from 0.01 to 100 or 0.01 to 500 W/m/K following ISO 22007-2 and GB/T 32064
• Transient Hot Wire (THW) Method for testing the absolute thermal conductivity, thermal diffusivity, specific heat of liquids, pastes & powders from 0.01 to 2 W/m/K. ASTM D7896
Transient Plane Source (TPS):
• Materials: Solids, Pastes and Powders
• Accuracy: 5 %
• Repeatability: 1 - 2 %
• Temperature: -75 °C to 300 °C (requires temperature chamber)
Temperature Chamber:
• Dry Bath: 0 to 100 °C
Included Testing Modules:
• TPS Standard - Bulk Module for measurement of low to high thermal conductivity materials
• TPS Slab - (avg radial), thermophysical properties of thermally conductive sheets
• Basic Thermal Conductivity: 0.01 to 100 W/m/K
• With optional Max Power Thermal Conductivity: 0.01 to 500 W/m/K
• Additional properties: Thermal Diffusivity, Volumetric Specific Heat, Thermal Effusivity
• Test Time: 2 to 160 seconds
• Sample Size: 10 x 10 mm to unlimited
• Sample Thickness: 0.01 mm to unlimited
• TPS Slab Sample: Smallest Sample: 15 x 15 x 0.1 mm
• Sample Configuration: Symmetric (Double-Sided), Asymmetric (Single-Sided)
• Stainless Steel 304 Verification Material
• Standard: ISO 22007-2, GB/T 32064
*Based on testing module used and sample properties
Transient Hot Wire (THW):
• Materials: Liquids, PCMs
• Thermal Conductivity: 0.01 to 2 W/m/K
• Temperature: -50 to 100 °C (requires temperature chamber)
• Additional Properties: Thermal Diffusivity, Volumetric Specific Heat
• Measurement Time: 1 second
• ASTM Standard: ASTM D7896-19
Temperature Chamber:
Dry Bath: 0 to 100 °C